IV curves obtained from thermionic emission tests with C12A7:e- thick film samples
Abstract
Thermionic emission current density measurement of C12A7:e- thick film samples.
Samples prepared by Fraunhofer IKTS.
Bulk coating: Proprietary composite with C12A7:e-. Thickness: 100 µm. Substrate: Titanium
Measurement conducted by Institute of Aerospace Engineering of TU Dresden.
URI
https://opara.zih.tu-dresden.de/xmlui/handle/123456789/5753http://dx.doi.org/10.25532/OPARA-193